Q. What is the basis of proportioning to ensure concrete of the desired weather resistance?

 

A. The w/cm to be selected for different types of structures for a wide variety of exposure conditions is given in ACI 211.1. For severe exposure conditions only air-entrained concrete is to be used. Where strength requirements indicate that lower w/cm are needed, the lower limits, of course, should govern.

 

References: SP-1(02); ACI PRC-211.1-22; ACI 212.3R-16