Q. What is structural low-density concrete? A. Structural low-density (lightweight) concrete is structural concrete made with low density aggregate having an air-dried density of not more than 115 lb/ft3 (1850 kg/m3) and a 28-day compressive strength of more than 2500 lb/in2 (17 MPa). References: SP-1(02); ACI 213R-14; E-1(16) Topics in Concrete: Aggregate; Concrete Fundamentals; Lightweight Concrete
Q. What is structural low-density concrete?
A. Structural low-density (lightweight) concrete is structural concrete made with low density aggregate having an air-dried density of not more than 115 lb/ft3 (1850 kg/m3) and a 28-day compressive strength of more than 2500 lb/in2 (17 MPa).
References: SP-1(02); ACI 213R-14; E-1(16)
Topics in Concrete: Aggregate; Concrete Fundamentals; Lightweight Concrete