Q. Do fibers react when added to a concrete mix? A. Unless the fibers are treated with specific chemicals that promote adhesion, fibers do not undergo a chemical reaction with the components of concrete. References: ACI 544.1R, ACI PRC-544.5 Topics in Concrete: Concrete Fundamentals, Fiber Reinforced Concrete
Q. Do fibers react when added to a concrete mix?
A. Unless the fibers are treated with specific chemicals that promote adhesion, fibers do not undergo a chemical reaction with the components of concrete.
References: ACI 544.1R, ACI PRC-544.5
Topics in Concrete: Concrete Fundamentals, Fiber Reinforced Concrete