A fiber manufacturer uses a proprietary design method. How can the validity of this method be confirmed?

In This Section

Other Sources for Answers

Search other resources on the ACI website for answers to technical questions

Technical Questions

ACI Committees, Membership, and Staff have answered common questions on a variety of concrete related topics.



A fiber manufacturer uses a proprietary design method. How can the validity of this method be confirmed?

Q. A fiber manufacturer uses a proprietary design method. How can the validity of this method be confirmed?

 

A. The validity of a proprietary design method for fiber-reinforced concrete can be confirmed using the design concepts and methods outlined in ACI 544.4R. These non-proprietary methods are based on peer-reviewed, published academic research and apply to all types of fibers, regardless of brand, material, or architecture. Design professionals can utilize ACI 544.4R to independently design or verify fiber-reinforced concrete calculations for any fiber type and application, ensuring consistency and validity.

 

References: ACI 544.1R, ACI 544.4R