Q. How is the abrasion resistance of concrete determined? A. Resistance to abrasion can be determined by ASTM C418, ASTM C779, and ASTM C944. References: SP-1(02); ACI 201.2R-16; ASTM C33; ASTM C418; ASTM C779; ASTM C944 Topics in Concrete: Durability; Pavement; Slab; Testing of Concrete
Q. How is the abrasion resistance of concrete determined?
A. Resistance to abrasion can be determined by ASTM C418, ASTM C779, and ASTM C944.
References: SP-1(02); ACI 201.2R-16; ASTM C33; ASTM C418; ASTM C779; ASTM C944