How is the abrasion resistance of concrete determined?

Q. How is the abrasion resistance of concrete determined?

 

A. Resistance to abrasion can be determined by ASTM C418, ASTM C779, and ASTM C944.

 

References: SP-1(02); ACI 201.2R-16; ASTM C33; ASTM C418; ASTM C779; ASTM C944

Topics in Concrete: Durability; Pavement; Slab; Testing of Concrete