Title: Chloride Threshold for Corrosion of Reinforcement in Concrete

Author(s): Syed Ehtesham Hussain, Ahmad S. Al-Gahtani, and Rasheeduzzafar

Publication: Materials Journal

Volume: 93

Issue: 6

Appears on pages(s): 534-538

Keywords: chlorides; corrosion; half-cell potential; porosity; reinforced concrete; reinforcing steels.

DOI: 10.14359/9857

Date: 11/1/1996

Abstract:
Cement mortar specimens made with three different C3A cements with a steel bar embedded centrally were partially immersed in a 5 percent NaCl solution, and half-cell potentials were monitored. When the potential value reached -270 mV versus saturated calomel electrode (SCE), taken as the threshold potential for the onset of corrosion of the embedded bar the specimens were taken out and pore solution extracted from the mortar sur-rounding the bar. The pore solutions were analyzed for Cl and OH con-centrations and threshold Cl/OH ratios computed. The threshold Cl-/OH ratio seemed to depend on the pore solution pH and was found to vary from 1.28 to 2.0 for a pore solution pH of 13.26 to 13.36. The free (water-soluble) chloride concentration in the pore solution was converted into threshold free chloride and total (acid-soluble) chloride contents. It was found that the threshold free chloride content was 0.22 to 0.29 percent by weight of cement and was independent of the C3A content of the cement. However, the threshold total chloride content was found to depend on the C3A con-tent of the cement and varied from 0.48 to 0.59, 0.73 to 0.85, and 1 .Ol to 1.20 percent for 2.43, 7.59, and 14 percent C3A cements, respectively.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer