Title: Impact Resistance of Steel Fiber Reinforced Concrete

Author(s): Nemkumar Banthia, Sidney Mindess, and J. - .F Trc

Publication: Materials Journal

Volume: 93

Issue: 5

Appears on pages(s): 472-479

Keywords: fiber reinforced concretes: impact; strength; tension: toughness.

DOI: 10.14359/9852

Date: 9/1/1996

Abstract:
Concrete in many civil engineering structures must have adequate resistance to impact and impulsively applied loads. Unfortunately, our understanding of the behavior of concrete to impact loads is far from adequate and there is significant variability in the published literature. The primary reason for this is the lack of a standardized technique of testing concrete under impact. This paper describes the construction of a simple impact machine capable of conducting impact test on concrete in uniaxial tension. Impact data for normal-strength, medium-strength, high-strength, and fiber reinforced concrete is presented. It is demonstrated that the machine is capable of generating rational impact data for various concretes tested and this data can be useful in design.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer