Title: Bond Strength of Noncontact Tension Lap Splices

Author(s): Bilal S. Hamad and Mohamad Y. Mansour

Publication: Structural Journal

Volume: 93

Issue: 3

Appears on pages(s): 316-326

Keywords: bond (concrete to reinforcement); development forced concrete; splice length; structural detailing; tests. length; rein-

DOI: 10.14359/9691

Date: 5/1/1996

Abstract:
The subject of transverse spacing between two reinforcing bars lapped in a noncontact or spaced tension splice is addressed in the ACI Building Code (ACI 318-89). The code provisions are based on monotonic tests performed before I957 of pullout specimens, beam-end specimens, and small-scale beam specimens, where the clear splice-bar spacing was small (less than 3 db or 50 mm). Tests reported in 1991 of full-scale flat plate specimens subjected to monotonic and repeated inelastic loading in direct tension did not check splice-bar spacings beyond the ACI Code limit of one-fifth of the required lap length. The study reported in this paper provides data on 17 full-scale slab specimens, each reinforced with three lap splices, loaded in flexure, and designed to fail in a splitting mode. Splice-bar spacings below and above the ACI limit were checked. The objective was to check the validity of the ACI provisions based on the results of this study and other studies of noncontact lap splices.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer