Title:
Design Durable Industrial Floor Slabs
Author(s):
Robert Fitzpatrick
Publication:
Concrete International
Volume:
18
Issue:
1
Appears on pages(s):
38-39
Keywords:
DOI:
Date:
1/1/1996
Abstract:
Concrete floor slabs on grade are inherently problematic. This article presents three of the common causes of problems with concrete floor slabs on grade and some "state of the art" innovations in floor slab design and construction that can reduce the occurrence of these problems.