Title: Fatigue Tests of Lightweight Aggregate Concrete Beams
Author(s): Harry A. Williams
Publication: Journal Proceedings
Volume: 39
Issue:
Appears on pages(s): 441-448
Keywords:
Date: 4/1/1943
Abstract:
Presents the results of a limited number of reversed and repeated loading tests of unreinforced concrete beams made with Haydite and Gravelite lightweight aggregates. True endurance limits were not deter- mined but the results give an indication of the en- durance strength for a limited number of repetitions.