Title: The Use of Carbon Dioxide to Reduce Efflorescence on Asbestos-Cement Shingles

Author(s): Clyde R. Hutchcroft and Harvey R. Anderson

Publication: Journal Proceedings

Volume: 37

Issue:

Appears on pages(s): 597-604

Keywords: none

Date: 4/1/1941

Abstract:
Describes experimental work with carbon dioxide gas to reduce efflorescence on asbestos-cement shin- gles. Factors investigated in connection with the reaction of carbon dioxide gas with the free lime of the shingles were: The effect of different arrangements of shingles for exposure to the carbon dioxide; the effect of the age and density of the shingles, concentrations of carbon dioxide gas, effect of temperature, moisture content, and of the depth to which the reactions occurred.




  

Please enter this 5 digit unlock code on the web page.