Title: Design of Light-Weight Zonolite Concrete Mixes
Author(s): Gregory P. Tschebotareff
Publication: Journal Proceedings
Volume: 37
Issue:
Appears on pages(s): 509-516
Keywords: none
Date: 2/1/1941
Abstract:
The results of a relatively limited number of tests with Iightweig ht Zonolite concrete mixes are given to illustrate peculiarities of such mixes which necessitate a special approach to the problem of their design. The investigation did not cover all of the factors which are likely to affect the properties of such liaht- weight briefly concretes, discussed . but some of these are listed and