Title: The Bond Between Concrete And Steel
Author(s): H. J. Gilkey, S. J. Chamberlin and R. W. Beal
Publication: Journal Proceedings
Volume: 35
Issue: 9
Appears on pages(s): 1-20
Keywords: none
Date: 9/1/1938
Abstract:
Reviews the subject of bond between concrete and steel, summarizing work of earlier investigators and presenting new data. Includes discussion, evaluation, and documentation; intended to answer questions for the designer and to raise questions for the investigator.