Title: High Early Strength Cement In Concrete Masonry Manufacture

Author(s): Benjamin Wilk

Publication: Journal Proceedings

Volume: 33

Issue: 3

Appears on pages(s): 499-502

Keywords: none

Date: 3/1/1937

Abstract:
Tests to determine the effect on durability of the reduced cement content when using high-early-strength cement are reported. The tests on freezing and thawing show that the reduced cement content does not reduce the resistance to freezing and thawing; the investigation of volume changes indi-cate that there is practically no difference between the shrinkage of high-early-strength cement concretes and normal cement concretes. The aggregate, however, had a marked effect.




  

Please enter this 5 digit unlock code on the web page.