Title: Testing Cast Stone

Author(s): ACI Committee 704

Publication: Journal Proceedings

Volume: 28

Issue: 9

Appears on pages(s): 33-36

Keywords: none

Date: 9/1/1931

Abstract:
Committee 704 reports on its test program concerning testing procedures and strength and density require-ments as covered by the Tentative Specification for Cast Stone (P3-A-29T) and recommends several changes in the specification.




  