Title: Properties Of Mass Concrete

Author(s): Raymond E. Davis and G. E. Troxell

Publication: Journal Proceedings

Volume: 27

Issue: 12

Appears on pages(s): 385-418

Keywords: none

Date: 12/1/1930

Abstract:
The total heat liberated by a given amount of cement from the time of beginning of hydration until hydration has been completed, can not readily be determined, but perhaps within ordinary limits of grinding may not differ as greatly with the chemical coposition of the cement as is sometimes supposed, even though the rate of heat generation during the early stages of hardening may be very much greater for one cement than for another




  