Title: Potomac Interceptor Sewer Tunnels and River Crossing Construciton

Author(s): John H. McGrann

Publication: Journal Proceedings

Volume: 62

Issue: 11

Appears on pages(s): 1363-1374

Keywords: ACI committee report, cement, concrete, nomenclature

Date: 11/1/1965

Abstract:
Describes construction features of a 3000 ft river crossing of a sewer line featuring 78 in. precast concrete pipe, and the 14,000 and 9000 ft tunnels at its ends. Pumping of the cast-in place tunnel linings is also described.




  