Title: Flexural Stiffness of Composite Columns Subjected to Bending about Minor Axis of Structural Steel Section Core

Author(s): S. Ali Mirza and Timo K. Tikka

Publication: Structural Journal

Volume: 96

Issue: 5

Appears on pages(s): 748-757

Keywords: building codes; columns (supports); composite construction (concrete and steel); concretes; loads (forces); moments; slenderness; steel; stiffness; structural design

DOI: 10.14359/728

Date: 9/1/1999

Abstract:
ACI 318-95 permits a moment magnifier approach for design of slender composite steel-concrete columns. This approach is strongly influenced by the effective flexural stiffness (EI) of the column that varies due to cracking, creep, and nonlinearity of the concrete stress-strain curve, among other factors. However, the EI expressions given in ACI 318-95 are approximate when compared with the values of EI computed from axial load-moment-curvature relationships. This study was undertaken to determine the influence of different variables on EI of slender, tied, rectangular composite columns in which steel shapes are encased in concrete. The columns studied were subjected to bending about the minor axis of the steel section in symmetrical sin-gle curvature under short-term loads. Approximately 12,000 simu-lated columns, each with a different combination of variables, were used to generate the stiffness data. The EI expressions were then developed for use in slender composite column designs. A design equation for EI is proposed.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer