Abstract:
A recent University of Toronto test of a 925 mm (36.4 in.) deep beam without stirrups showed a shear strength vc that is only slightly below the value vc = 2vfc' required by ACI 318-08, and comfortably above the value f × 2vfc' (where f = 0.75 is the sstrength reduction factor, and vc and fc' are in psi). On that basis, and in view of the safety provisions of the Code, it is often thought that the current shear strength provisions for beams up to 0.2 m (8 in.) deep, which neglects the size effect, are safe for beams up to 1 m (40 in.) deep. This is not true, however, for it must be expected that if numerous tests of 1 m (40 in.) deep beams with different shear spans and steel ratios, made of different concretes and under different hygro-thermal conditions, could be carried out, the beam strength would exhibit a similar statistical scatter, with approximately the same coefficient of variation (CoV), as the strength of beams up to 0.2 m (8 in.) deep, for which there are numerous test results in the database. Based on this expected scatter, it is shown that neglecting the size effect for beams up to 1 m (40 in.) deep is likely to increase the expected frequency of failures from approximately 1 in a million to approximately 1 in a thousand when the beam depth increases from 0.2 to 1 m (8 to 40 in.).


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer