Title: Solidification and Stabilization of Waste Using Portland Cement

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 16

Keywords: waste

Date: 10/1/1994

Abstract:
State-of-the-art report on the characteristics of Portland cement and how it can be used effectively to solidify / stabilize various types of wastes. Discusses waste compounds that may interfere with cement hydration reactions. Includes information on several additives that may be used with Portland cement to enhance solidification / stabilization reactions.




  