Title: 503.6R-97: Guide for the Application of Epoxy and Latex Adhesives for Bonding Freshly Mixed and Hardened Concretes (Reapproved 2003)
Author(s):
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s): 4
Keywords: epoxies
Date: 9/24/1997
Abstract:
Note: A newer version of this document exists. This document was replaced by 548.11R-12.
Note: 503.6R-97 is only available in PDF format.
The objective of this guide is to provide information, requirements, and procedures necessary to achieve a bond between freshly-mixed and hardened concretes by use of either epoxy or latex adhesives. The requirements and procedures of this guide consist of: Evaluation of the hardened concrete to determine the proper preparation and surface conditioning prior to application adhesive depending on the expected performance and environmental conditions; application method.