Title:
ACI PRC-213-14(23) Guide for Structural Lightweight-Aggregate Concrete Reapproved 2023
Author(s):
ACI Committee 213
Publication:
Technical Documents
Volume:
Issue:
Appears on pages(s):
53
Keywords:
DOI:
Date:
2/1/2024
Abstract:
The guide summarizes the present state of technology, presents and interprets the data on lightweight-aggregate concrete from many laboratory studies and the accumulated experience resulting from its successful use, and reviews performance of structural lightweight aggregate concrete in service. This guide includes a definition of lightweight-aggregate concrete for structural purposes and discusses, in a condensed fashion, the production methods for and inherent properties of structural lightweight aggregates. Current practices for proportioning, mixing, transporting, and placing; properties of hardened concrete; and the design of structural concrete with reference to ACI 318 are all discussed.
Keywords: abrasion resistance; aggregate; bond; contact zone; durability; fire resistance; internal curing; lightweight aggregate; lightweight concrete; mixture proportion; shear; shrinkage; specified density concrete; strength; thermal conductivity