Abstract:
Three-dimensional (3-D) printed concrete is a new technology for civil engineering. In this paper, 3-D printed concrete was prepared for a study on static and dynamic properties. The best fluidity of the concrete was researched and the optimization mixture ratio for better mechanical performance was discussed. The mechanical performances of the concrete were tested and the anisotropy phenomenon in 3-D printed concrete was found. The computed tomography (CT) scanning and imaging progress methods were used to discuss the reason for the phenomenon. The penetration experiments were carried out to research the dynamic performance of the 3-D printed concrete. The results of the penetration tests were compared with the empirical formulas. The Young formula was improved according to the results.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer