Title: Durability of Concrete Containing Liquid Crystal Display Glass Powder for Pavement

Author(s): Ilhwan You, Goangseup Zi, Doo-Yeol Yoo, and David A. Lange

Publication: Materials Journal

Volume: 116

Issue: 6

Appears on pages(s): 87-94

Keywords: cement replacement; concrete pavement; durability; liquid crystal display glass powder; pozzolanic admixture

DOI: 10.14359/51716814

Date: 11/1/2019

Abstract:
This paper describes the feasibility of using waste liquid crystal display glass powder (LCDP) as a partial cement replacement in concrete for pavements. The chemical and physical properties of LCDP are investigated and discussed for considering its use as a pozzolanic admixture. To evaluate the performance of concrete pavement incorporating LCDP, the mechanical and durability properties in terms of the resistance to abrasion, alkali-silica reaction, chloride penetration, and freezing and thawing are investigated. The results indicate that LCDP has suitable chemical and physical properties that satisfy the requirements of the Class F pozzolanic admixture in the ASTM standard. Thanks to very low alkali content and many amorphous forms of alumina, the incorporation of LCDP significantly improves the resistance to alkali-silica reaction and penetration of chloride ions. In addition, concrete containing LCDP also shows similar strength development at later ages and similar resistance to freezing and thawing compared to fly ash concrete.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer