Title: Behaviour of the prestressed concrete submitted to thermal cycles from atmospheric temperatures to - 165ºC

Author(s): Corres Peiretti, H.; Planas Rosselló, J.; Elices Calafat, M.

Publication: ACHE

Volume: 36

Issue: 154

Appears on pages(s): 219 -

Keywords:

Date: 1/1/1985

Abstract:


ACI International Partner, ACHE Spain, International Partner Access.