Title: Bridge over the Daró river, in the bypass of La Bisbal d´Empordà

Author(s): Roig Vilaseca, J. Mª

Publication: ACHE

Volume: 57

Issue: 242

Appears on pages(s): 6 -

Keywords:

Date: 1/8/2006

Abstract:
A composite deck over the Daró River in La Bisbal d?Empordà (46.7 m span and 12.4 m width) is exposed. The adopted structural typology combines the existing technical determinants (clearance, the bridge abutement support conditions and the drainage capacity) with an appropiate integration of the structure in the urban environment and a good aesthetic quality.


ACI International Partner, ACHE Spain, International Partner Access.

View Resource »