Title: Durability of Rapid-Strength Concrete Produced with Ettringite-Based Binders

Author(s): Edward G. Moffatt and Michael D. A. Thomas

Publication: Materials Journal

Volume: 115

Issue: 1

Appears on pages(s): 105-115

Keywords: calcium aluminate cement; calcium sulfoaluminate cement; carbonation; chloride ingress; corrosion; durability; linear polarization; scaling resistance

DOI: 10.14359/51701006

Date: 1/1/2018

Abstract:
Rapid-strength concretes are currently used to repair structures such as bridge decks, substructure elements on bridges (for example, piers and columns), pavements, and components of buildings. Although these products gain a high strength in a short period of time (for example, ≥ 20 MPa [3000 psi] in 3 hours), it is usually intended that they not only provide a temporary fix but can also provide a permanent repair for the remaining service life of the structure. One approach for delivering high early-age strength is through the rapid formation of ettringite using a binder that contains a calcium aluminate or calcium sulfoaluminate phase with calcium sulfate. Although it has been proven that such binders gain high early strength and acceptable working time, limited information exists concerning the long-term durability of concrete produced with these binders in the aggressive conditions often encountered in service. This paper presents durability data on the chloride resistance, corrosion protection properties, deicer salt scaling and carbonation resistance. These concretes include: portland cement (PC) and high-early-strength portland cement (HEPC) as references; a newly developed ternary cement (PC-CAC-CS) consisting of a blend of PC, calcium aluminate cement (CAC), and calcium sulfate (CS); and two commercially available calcium-sulfoaluminate (CSA) cement systems.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer