Experimental Determination of Cohesion and Internal Friction Angle on Conventional Concretes

International Concrete Abstracts Portal

  


Title: Experimental Determination of Cohesion and Internal Friction Angle on Conventional Concretes

Author(s): Selim Pul, Amir Ghaffari, Ertekin Oztekin, Metin Hüsem, and Serhat Demir

Publication: Materials Journal

Volume: 114

Issue: 3

Appears on pages(s): 407-416

Keywords: cohesion; conventional concrete; direct shear test; Drucker-Prager parameters; internal friction angle; Mohr-Coulomb failure criterion; nonlinear finite element analysis

DOI: 10.14359/51689676

Date: 5/1/2017

Abstract:
Various failure criterions have been used for the nonlinear analysis of concrete and reinforced concrete structures. To get more accurate results from the analyses, the selected failure criterion must be appropriate with the characteristics of problem and the assumptions made in the criterion should comply with the characteristics of problem. In this study, an experimental investigation was carried out to determine the cohesion (c) and internal friction angle (ϕ) values, which are in the compressive strength range of 14.4 MPa ≤ fcm cube ≤ 47.0 MPa (2.03 ksi ≤ fcm cube ≤ 6.82 ksi) that are used in failure criterions such as Mohr-Coulomb and Drucker-Prager preferred in end unit analyses for concrete and reinforced concrete structures. Tests are performed by using the direct shear test system, which is designed and produced for this study. Finally, cohesion and internal friction angle were determined between 2.94 and 12.34 MPa (0.43 and 1.79 ksi) and 29.8 and 41.7 degrees, respectively.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer