Title: Effect of Low-Temperature Installation on Adhesive Anchors

Author(s): Werner Fuchs, Jan Hofmann, and Gerrit Hülder

Publication: Concrete International

Volume: 38

Issue: 1

Appears on pages(s): 48-56

Keywords: curing, conversion, load, stiffness

Date: 1/1/2016

Abstract:
Until recently, the behavior of adhesive anchors installed in cold concrete components was inadequately investigated. The article presents background information on the load-bearing behavior of adhesive anchors installed at low temperatures, describes corresponding tests, and reports test results. These results indicate that the behavior of low-temperature installation of adhesive anchor products is sufficiently considered in the product prequalification provisions now specified in the United States.