Title: INVERTED-T BEAMS: EXPERIMENTS AND STRUT-AND-TIE MODELING

Author(s): N. L. Varney, E. Fernández-Gómez, D. B. Garber, W. M. Ghannoum, and O. Bayrak

Publication: Structural Journal

Volume: 112

Issue: 2

Appears on pages(s): 147-156

Keywords: D-region; inverted-T beam; laboratory testing; large-scale; nonlinear design; reinforced concrete; shear; shear span; strut-and-tie.

DOI: 10.14359/51687403

Date: 3/1/2015

Abstract:
Contrary to rectangular deep beams, inverted-T beams are loaded on a ledge at the bottom chord of the beam. This loading configuration induces a tension field into the web and the resulting complex strain distribution renders sectional design provisions inadequate. The applicability of strut-and-tie modeling (STM), developed for rectangular deep beams and simpler, two-dimensional designs, was evaluated. An experimental study was conducted in which 33 tests were performed on 22 large-scale reinforced concrete inverted-T beams and the effects of the following variables were investigated: ledge geometry, quantity of web reinforcement, number of point loads, member depth, and shear span-depth ratio. It was concluded that strut-and-tie modeling, although developed for much simpler structural components, offers a simple and accurate design method for the more complex strain distributions in inverted-T beams. The STM provisions developed for rectangular beams accurately captured both failure mode and ultimate capacity and are recommended for use in inverted-T beam design, as a major conclusion of this research.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer