Title: Effectiveness of Steel Fiber as Minimum Shear Reinforcement

Author(s): Jimmy Susetyo, Paul Gauvreau, and Frank J. Vecchio

Publication: Structural Journal

Volume: 108

Issue: 4

Appears on pages(s): 488-496

Keywords: crack control; ductility; panel tests; reinforcement; shear; steel fiber; strength

DOI: 10.14359/51682990

Date: 7/1/2011

Abstract:
Ten 35 x 35 x 2.75 in. (890 x 890 x 70 mm) concrete panels were tested under in-plane pure-shear monotonic loading conditions to evaluate the effectiveness of steel fibers in meeting minimum shear reinforcement requirements for concrete elements. The test results indicate that concrete elements exhibiting ductile behavior, sufficient shear strength, and good crack control characteristics can be obtained with an adequate addition of steel fibers, meeting or exceeding the level of performance achievable using codeprescribed minimum amounts of conventional shear reinforcement. Fiber aspect ratio, fiber length, fiber tensile strength, fiber volume content, and concrete compressive strength are found to influence the shear performance of fiber-reinforced concrete (FRC) to varying extents. Details and results are provided.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer