Title: Fiber Reinforced Concrete for Exterior Slabs-on-Grade, Part I

Author(s): Jean-francois Trottier, Dudley R. Morgan, and Dean Forgeron

Publication: Concrete International

Volume: 19

Issue: 6

Appears on pages(s): 35-39

Keywords: air entrainment; compressive strength; fiber reinforced concretes; flexural strength; metal fibers; slabs;

DOI:

Date: 6/1/1997

Abstract:
The influence of fiber type and fiber geometry on the fresh and hardened properties of ready-mix produced fiber reinforced concrete for exterior slab on grade applications was studied. Four commercially available steel fibers were investigated. This study indicated that the addition of steel fibers at 0.5 percent by volume did not significantly modify the characteristics of the hardened air-void system of the concrete. This study also demonstrated that the fiber geometry and the type of fiber used have a significant influence on the flexural toughness of the composite while other properties such as compressive and flexural strength remain relatively unaffected.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer