Title: Application Mechanism of Silane Weatherproofers

Author(s): Edward McGettigan

Publication: Concrete International

Volume: 12

Issue: 10

Appears on pages(s): 66-68

Keywords: absorption; chemical analysis; concretes; evaporation; moisture content; porosity; silanes; waterproofing; weatherproofing; General

DOI:

Date: 10/1/1990

Abstract:
To rectify inaccuracies concerning the volatility of silanes and their application under harsh conditions, a study was undertaken that included analysis of the chemical and physical-chemical interactions that accompany application, laboratory evaluation of absorption and evaporation rates, and test applications under harsh environmental conditions. Results show that forces such as capillary action, electrochemical attraction, and chemical reaction occur so quickly that the effect of volatility is insignificant.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer