Premixed Cement Paste

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Premixed Cement Paste

Author(s): Gary R. Mass

Publication: Concrete International

Volume: 11

Issue: 11

Appears on pages(s): 82-85

Keywords: cement pastes; compressive strength; concretes; premixing; evaluation performance; portland cements; Manufacturing

Date: 11/1/1989

Abstract:
The results of a study made to compare the compressive strength of conventionally mixed concrete with that of concrete containing premixed cement paste are presented. The work was performed with samples from commercial ready-mixed concrete production. The plant setup, materials, and mixtures are described. Evaluation of data shows specific parameters are necessary for optimum performance.