Title: Modeling the Thermal Stresses at Early Ages in a Concrete Monolith

Author(s): Eric Ayotte, Bruno Massicotte, Jules Houde, and Vladimir Gocevski

Publication: Materials Journal

Volume: 94

Issue: 6

Appears on pages(s): 577-587

Keywords: dams; freeze thaw durability; heat of hydration; mass concrete; modeling; strains; stresses;

DOI: 10.14359/342

Date: 11/1/1997

Abstract:
This paper presents details of an experimental and numerical study of thermal strains and induced stresses in large-scale mass concrete. Three large-scale monoliths were built on a dam construction site in the James Bay Territory to monitor the thermal behavior of mass concrete subjected first to heat of hydration development and subsequent freeze and thaw cycles. The monoliths were instrumented with thermocouples and mechanical strain gages. The modeling of one monolith was carried out with the computer program ADINA. The modeling includes the development of a heat of hydration curve typical to the concrete used in dam construction. The mechanical properties of early-age concrete were based on measurements or evaluated from various references. It is shown that, due to an inadequate representation of the reference temperature, many nonlinear incremental commercial software systems cannot correctly simulate the stress history of maturing concrete with the temperature variation. The paper presents a modified step-by-step approach which improved the stress modeling within the available commercial software. Excellent agreement between measured and computed temperatures and stresses was obtained.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer