Title: Collapse of Danish Prestressed Tanks

Author(s): Troels Brøndum-nielsen

Publication: Concrete International

Volume: 21

Issue: 4

Appears on pages(s): 55-56

Keywords: buckling; collapse; cylindrical shells; instability; prestressed concrete; tanks; stability

DOI:

Date: 4/1/1999

Abstract:
A considerable number of tendon stressed tanks, representing a particular tank design practiced in Denmark, have collapsed in recent years. The tanks were constructed of precast concrete wall panels erected on an in situ base slab. The tanks were post-tensioned by exterior unbonded circumferential tendons, threaded through holes in the buttresses along the vertical wall joints. The collapses occurred during tensioning, up to a maximum four hours later; these collapses were limited to tanks with a large number of wall panels (about 40 to 64).




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer