Title: Effect of Longitudinal Tensile Reinforcement Ratio and Shear Span-Depth Ratio on Minimum Shear Reinforcement in Beams

Author(s): Jung-Yoon Lee and Uk-Yeon Kim

Publication: Structural Journal

Volume: 105

Issue: 2

Appears on pages(s): 134-144

Keywords: beams; high-strength concrete; reinforced concrete; shear reinforcement; span; tensile reinforcement.

DOI: 10.14359/19728

Date: 3/1/2008

Abstract:
This paper presents the effects of longitudinal tensile reinforcement ratio and shear span-depth ratio (a /d) on the minimum shear reinforcement in reinforced concrete beams. Twenty-six reinforced concrete (RC) beams having the minimum shear reinforcements required by ACI 318-05 were cast, instrumented, and tested. Although the minimum amount of shear reinforcement in the existing design codes (ACI 318-05, CSA A23.3-04, AIJ-99, and Eurocode 2) depend on neither the longitudinal tensile reinforcement ratio nor the a/d, the test results indicated that the reserve shear (shear strength of the beam with minimum amount of shear reinforcement/shear strength of the beam without shear reinforcement) of the tested beams increased as the longitudinal tensile reinforcement ratio increased, but decreased as the a/d increased.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer