Title: Safe Shear Design of Large Wide Beams
Author(s): Lubell, A. S.; Sherwood, E. G.; Bentz, E. C.; and Collins, M. P.
Publication: 318Reference
Volume: 11
Issue: 22
Appears on pages(s): pp. 66-78.
Keywords:
Date: 6/1/2008
Abstract:
Concrete International, V. 26, No. 1, Jan. 2004