Title: Shear Transfer By Aggregate Interlock

Author(s): T. Paulay and P.J. Loeber

Publication: Symposium Paper

Volume: 42

Issue:

Appears on pages(s): 1-16

Keywords: aggregate interlock; aggregate shape and texture; beams (supports); concretes; crack width and spacing; cracking (fracturing) cyclic loads; joints (junctions); shear stress; stiffness; stress transfer; stresses; tests

Date: 1/1/1974

Abstract:
In a test program, comprising 44 speciments, the nature of shear transfer across prepared cracks by aggregate interlock mechanism was further explored.




  