Ultimate Strength of Reinforced Concrete Grid and Slab Bridges

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Ultimate Strength of Reinforced Concrete Grid and Slab Bridges

Author(s): S.U. Pillai and S.D. Lash

Publication: Symposium Paper

Volume: 23

Issue:

Appears on pages(s): 361-384

Keywords: beams (structural); bridge decks; bridges (structures); concrete slabs; continuity (structural); deflection; flexural strength; limit design method (structural); linear programming; minimization; moments; optimization; plastic analysis (structural)

Date: 1/1/1969

Abstract:
A method based on plastic theory and including torsional resistance is described for estimating the ultimate load of medium-span reinforced concrete grid and slab bridges.




  