The Role of Shrinkage-Compensating Cement in Reduction of Cracking of Concrete

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: The Role of Shrinkage-Compensating Cement in Reduction of Cracking of Concrete

Author(s): J.A. Hanson, Richard C. Elstner, Robert H. Clore

Publication: Symposium Paper

Volume: 38

Issue:

Appears on pages(s): 251-272

Keywords: compressive strength; concretes; cracking (fracturing); creep properties; drying shrinkage; expansion; expansive cement type M: modulus of elasticity; restraints; shrinkage; shrinkage-compensating concretes; slump tests; splitting tensile strength

Date: 1/1/1973

Abstract:
Concretes containing Type M shrinkage-compensating cement were compared in the laboratory with those containing Type I portland cement.




  