Title: Transverse Load Capacity of Multi-Dowel Anchorages in Concrete

Author(s): Julius G. Potyondy

Publication: Special Publication

Volume: 103

Issue:

Appears on pages(s): 283-296

Keywords: anchors (fasteners); bolts; concretes; dowels; embedment; loads (forces); structural design; Design

Date: 9/1/1987

Abstract:
A detailed research program in presented on cast-in-place anchorages in concrete. Single and multidowel units were tested under transverse loads with variable moment arms. The strain distribution along the embedded anchors was measured to determine the re