Elastomeric Bearing Pad Connections in Precast Concrete Parking Structures
Author(s):
James R. Libby
Publication:
Concrete International
Volume:
9
Issue:
9
Appears on pages(s):
50-58
Keywords:
bearings; connections; parking structures; precast concrete; plastics, polymers and resins; Design
DOI:
Date:
9/1/1987
Abstract:
Describes four instances of failure of elastomeric bearing pad connections in precast concrete parking structures. Areas needing research are enumerated and design and specification standards are called for.