Title: A Study of Hooked Bar Anchorages in Beam-Column Joints

Author(s): Jirsa, J. O., and Marques, J. L. G.

Publication: 318Reference

Volume: 12

Issue: 13

Appears on pages(s): pp. 198-200.

Keywords:

Date: 6/1/2008

Abstract:
ACI JOURNAL, Proceedings V. 72, No. 5, May 1975