Shear Transfer in Concrete Having Reinforcement at an Angle to the Shear Plane

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Shear Transfer in Concrete Having Reinforcement at an Angle to the Shear Plane

Author(s): Mattock, A. H.

Publication: 318Reference

Volume: 11

Issue: 46

Appears on pages(s): pp. 17-42.

Keywords:

Date: 6/1/2008

Abstract:
Shear in Reinforced Concrete, SP-42, American Concrete Institute, Farmington Hills, MI, 1974


Free Access

View Resource »  



  