Title: Report of Committee on Testing Cement and Cement Products

Author(s): E.S. Larned, Chariman

Publication: Journal Proceedings

Volume: 5

Issue: 1

Appears on pages(s): 484-494

Keywords: none

Date: 1/1/1909

Abstract:
In considering material for the annual report of this Committee, it was deemed an opportune time to invite some form of original research work, for which each member is specially equipped by reason of long experience and responsible connection with an established laboratory of recognized authority.




  