Title: Report of Committee on Reinforced Concrete

Author(s): Sanford E. Thompson, Chairman

Publication: Journal Proceedings

Volume: 5

Issue: 1

Appears on pages(s): 454-474

Keywords: none

Date: 1/1/1909

Abstract:
The recommendations in this report conform in general to the more complete report of the Joint Committee on Concrete and Reinforced Concrete representing the American Society of Civil Engineers, the American Society for Testing Materials, the American Railway Engineering and Maintence of Way Manufacturers. The same unit stresses are suggested and the formulas are based on these unit stresses using methods of computation advised by the Joint Committee.




  

Please enter this 5 digit unlock code on the web page.