Title: Reinforced and Plain Concrete Sewers and Conduits
Author(s): ACI Committee S-3
Publication: Journal Proceedings
Volume: 19
Issue: 1
Appears on pages(s): 428
Keywords: none
Date: 1/1/1923
Abstract:
Committee S-3, on Reinforced and Plain Concrete Sewers and Conduits submits herewith an appendix to the "Standard Specifications for Monolithic Concrete Sewers, Reinforced Concrete Pipe Sewer, with Recommended Rules for Concrete Sewer Design, revised in 1920."