Title: Tenative Recommended Practice and Standard Specfications for Concrete Fuel Oil Tanks
Author(s): ACI Committee S-4
Publication: Journal Proceedings
Volume: 19
Issue: 1
Appears on pages(s): 420-427
Keywords: none
Date: 1/1/1923
Abstract:
Concrete tanks are recommended for the storage of fuel oil when the specific gravity of the liquid is heavier than 35 degree Baume at 60 degree Fahrenheit, but should not ordinarily be used for lighter oils.